    Ultrasonic vs Radiographic Testing of Girder Welds

    Compare ultrasonic and radiographic testing for bridge girder welds, with joint examples, access requirements and a checklist for reviewing inspection reports.

    Author
    Kothari Chemicals (Engineering Division)
    Last updated
    Last updated: 23 November 2026
    Reading time
    5 min read

    Ultrasonic testing (UT) and radiographic testing (RT) both examine the interior of a girder weld. UT uses sound reflections to locate indications within the steel. RT produces an image of changes in attenuation through the joint. The inspection and test plan (ITP) should identify the required method, coverage and acceptance criteria for each weld before fabrication begins.

    Consider a transverse butt splice joining two flange plates. The drawing identifies the joint and its dimensions, the weld schedule identifies the weld, and the ITP calls up the examination and acceptance requirements. Reviewing those documents together lets the fabrication and inspection teams check whether the finished splice will provide the access that the approved technique requires.

    What ultrasonic testing can show

    An ultrasonic probe sends sound into the steel. In an angle-beam examination, a technician moves the probe along the plate to cover the specified weld volume. The position of the probe and the return time of the echo help locate an indication along the joint and through the thickness. A suitably directed beam can respond strongly to a planar discontinuity such as lack of fusion. The same discontinuity may produce a much weaker response at another angle.

    The technician needs a suitable scan surface, space to move the probe and a defined way to check the instrument response against a reference block. A stiffener close to a weld can restrict probe travel. Review those obstructions before fixing the fabrication sequence so the team can preserve access or submit a revised examination plan for approval.

    What radiographic testing can show

    RT uses an X-ray or gamma-ray source and film or a digital detector on the opposite side of the joint. The resulting projection can make volumetric discontinuities such as porosity visible. Tight planar discontinuities can be harder to resolve when their orientation provides little contrast. A single projection also gives limited information about the indication's depth.

    The approved technique identifies how exposures cover the weld and how image quality is verified. Ask for the image identifier, the weld location covered and the evidence from the required image quality indicator (IQI). Plan space for the source and detector and schedule the work around the radiation safety controls required for the exposure.

    Comparing UT and RT during fabrication

    DecisionUltrasonic testingRadiographic testing
    AccessRoom for probe movement on the scan surfaces specified in the procedureSpace for source and detector placement on opposite sides and for a controlled radiation area
    Indication informationPosition and estimated depth where the approved technique supports itProjection showing the position and extent visible on the image
    Typical sensitivityPlanar reflectors can give a strong response at a suitable beam anglePorosity and other volumetric discontinuities can show clear image contrast
    Record to requestWeld map reference, scan coverage, results and any required scan dataExposure map, images, image-quality evidence and interpretation report

    The FHWA Bridge Welding Reference Manual, chapter 6 explains the methods and their limitations. Use the governing project documents to establish which methods apply to your girder package.

    Plan weld inspection before access closes

    • Flange or web butt splice. Check the governing joint-specific requirements first. If UT is specified, verify the scan path and surfaces. If RT is specified, verify source and detector access and plan how the exposures will cover the splice. Some contracts require more than one method on the same joint.
    • Full-penetration tee joint near a stiffener. Have the inspection team review the actual joint detail and adjacent steelwork. Schedule examination before later assembly obstructs the approved scan path where the fabrication and inspection plans allow it.
    • Fillet weld or suspected surface crack. Start with the visual and surface examination requirements for that joint. See the guide to dye penetrant and magnetic particle testing for how those methods address surface indications.

    What to check before signing off a report

    1. Traceability. The member mark, weld ID and drawing revision match the latest approved weld map. A datum or marked start point lets another inspector find the same location.
    2. Coverage. The report shows which weld lengths or volumes were examined and records any restricted or unexamined areas. Compare the recorded coverage to what the ITP requires.
    3. Evaluation. The method, written procedure revision, examiner qualification and acceptance reference are identified. The reviewer can follow how each reportable indication was evaluated.
    4. Repair history. If a weld was repaired, the re-examination record identifies the repair location and links back to the original indication and its disposition.
    5. Release. Any required witness or hold-point sign-off is recorded before the member moves to the next operation.

    Kothari Chemicals (Engineering Division) lists UT and RT among its inspection capabilities. For a quote, send the girder drawings, weld schedule and inspection requirements. See the steel fabrication quality-control guide for how weld reports fit into the wider quality records.

    Frequently asked questions

    Can UT replace RT on a bridge girder splice?

    A substitution requires permission under the governing project documents and any approval they specify. Ask the responsible authority to confirm the revised method and coverage in the ITP before work proceeds.

    Does every indication require repair?

    The examiner evaluates reportable indications against the acceptance criteria for the joint. The resulting disposition determines whether the weld can be accepted, needs repair or requires further review.

    What is the difference between the test procedure and the acceptance criteria?

    The procedure describes how the examination is performed and recorded. The acceptance criteria set the limits used to evaluate indications for that project. The ITP should identify the applicable reference and edition for each.

    • NDT
    • ultrasonic testing
    • radiographic testing
    • girder welds
    • quality control

    About Kothari Chemicals (Engineering Division)

    The Kothari Chemicals (Engineering Division) at Kothari Chemicals (Engineering Division) writes from day-to-day work in steel fabrication, quality assurance and project execution at the Bhilai works.

    Enquiries

    Send your drawings for a technical review.

    Share drawings, specifications, quantities and delivery requirements. Our engineering team reviews scope, inspection needs and schedule before quoting.

    Works & sales
    +91 788 2974 016
    Hours
    Mon–Sat, 9:00–18:00 IST
    Works
    Plot No. 3, Heavy Industrial Area, Hathkhoj, Bhilai 490026, Chhattisgarh, India